Cracking/Exploding

Read this tip to make your life smarter, better, faster and wiser. LifeTips is the place to go when you need to know about Handbuilt and other Ceramics topics.

Have I allowed enough time for carbon burnout?

Cracking/Exploding

Have I allowed enough time for carbon burnout?
It is important to burn out all carbon from the ware before higher temperatures are reached (1200°F or 650°C). It takes time for oxygen to move into the pourous body, react with the carbon and then leave. If carbon remains, many problems can occur. These include problems with colour, glaze fit, strength, blistering and discolouration. Use of a downdraft vent system, combined with slower heating, virtually eliminates carbon related problems.

   