Recognizing Under Deflocculation
If the slip is gelling after a few minutes or livering while mixing, more deflocculant is probably needed. Be careful not to add too much; this is a common mistake and will mean you will have to make more of the powder mix and add it and more water to counterbalance the oversupply of deflocculant. If the slip does not settle out overnight, then you can rest easy, it is not over deflocculated.
If the slip has not thinned after an addition, then there is already enough present. Sometimes a very small addition of water will thin the slip dramatically.

About LifeTips

Now one of the top on-line publishers in the world, LifeTips offers tips to millions of monthly visitors. Our mission mission is to make your life smarter, better, faster and wiser. Expert writers earn dough for what they know. And exclusive sponsors in each niche topic help us make-it-all happen.

Not finding the advice and tips you need on this Ceramics Tip Site? Request a Tip Now!


Guru Spotlight
Byron White